Mold that ready for pouring process.

Furnace.

Finished Product.

Bottom view, right top is the pouring hole.
Casting defect: Flow line.

Side view.
Casting defect: Flow line.

Top of the Finished Product.
Ruler used to show another casting defect, sink mark.

Done! Anyone interested in changing major to Mechanical Engineering or decided to take Mechanical Engineering as major?
3 comments:
Did you enjoy yourself working on the project? If you did, then good. If you didn't, then its time to really consider changing major.
FYI, the defects such as sink mark and flow line, are quality issues. For every defect, there is a dollar amount associated with it. And here's when IE comes into the picture. :)
If I'm not enjoying the class then I wont post it up here. HAHA!
O!
Mine project is low cost project so for sure will come with plenty of deflect.
Low budget does not necessary mean low quality. In fact, corporations strive to attain high quality and keep the cost low at the same time. Low cost <> low quality. Keep this in mind for whatever you do.